Resistance tabo walda tsari na beryllium jan karfe

Beryllium jan ƙarfe yana da ƙananan juriya, mafi girman ƙarfin zafin jiki da haɓaka haɓaka fiye da ƙarfe.Gabaɗaya, jan ƙarfe na beryllium yana da ƙarfi iri ɗaya ko mafi girma fiye da ƙarfe.Lokacin amfani da juriya tabo waldi (RSW) beryllium jan karfe kanta ko beryllium jan karfe da sauran gami, yi amfani da mafi girma waldi halin yanzu, (15%), ƙananan ƙarfin lantarki (75%) da guntu waldi lokaci (50%) .Tagulla na Beryllium yana jure matsi mafi girma na walda fiye da sauran kayan haɗin ƙarfe, amma matsalolin kuma na iya haifar da matsalolin da suka yi ƙasa da yawa.
Don samun daidaiton sakamako a cikin gami da jan ƙarfe, kayan walda dole ne su sami ikon sarrafa daidai lokaci da na yanzu, kuma an fi son kayan walda AC saboda ƙananan zafin wutar lantarki da ƙarancin farashi.Lokacin walda na 4-8 hawan keke ya haifar da sakamako mai kyau.Lokacin walda karafa masu irin wannan na'urorin haɓakawa, karkatar walda da walda mai wuce gona da iri na iya sarrafa faɗaɗa ƙarfen don iyakance ɓoyayyiyar haɗarin fashewar walda.Beryllium jan karfe da sauran na'urorin tagulla ana walda su ba tare da karkatar da walda ba.Idan an yi amfani da walƙiya mai ƙima da walƙiya mai jujjuyawa, adadin lokutan ya dogara da kauri na kayan aikin.
A cikin juriya tabo walda beryllium jan karfe da karfe, ko wasu high juriya gami, mafi kyau thermal ma'auni za a iya samu ta amfani da lantarki tare da karami lamba saman a kan beryllium jan karfe gefen.Kayan lantarki da ke hulɗa da jan ƙarfe na beryllium ya kamata ya kasance yana da ƙarfin aiki mafi girma fiye da aikin aiki, lambar ƙirar ƙungiyar RWMA2 ta dace.Ƙarfe masu jujjuyawa (tungsten da molybdenum) suna da manyan wuraren narkewa.Babu wani hali don tsayawa ga jan karfe na beryllium.13 da 14 pole electrodes kuma akwai.Amfanin karafa masu jujjuyawa shine tsawon rayuwarsu.Duk da haka, saboda taurin irin waɗannan allunan, lalacewar ƙasa na iya yiwuwa.Na'urorin sanyaya ruwa zasu taimaka sarrafa zafin jiki da tsawaita rayuwar lantarki.Koyaya, lokacin walda sassan siraran ƙarfe na beryllium jan ƙarfe, amfani da na'urorin sanyaya ruwa na iya haifar da kashe ƙarfen.
Idan kauri bambanci tsakanin beryllium jan karfe da high resistivity gami ya fi 5, tsinkaya walda ya kamata a yi amfani da saboda wahalar practicable thermal ma'auni.
Juriya tsinkayar waldi
Yawancin matsalolin jan karfe na beryllium a cikin juriya tabo waldi za a iya magance su tare da juriya tsinkayar waldi (RPW).Saboda ƙananan yankin da zafi ya shafa, ana iya yin ayyuka da yawa.Karfe daban-daban na kauri daban-daban suna da sauƙin waldawa.Ana amfani da na'urori masu faɗin ɓangaren giciye da nau'ikan nau'ikan lantarki daban-daban a cikin juriya na tsinkayar walda don rage lalacewa da mannewa.Ƙarƙashin wutar lantarki ba shi da matsala fiye da na juriya ta walda.Abubuwan da aka fi amfani da su sune 2, 3, da 4 pole electrodes;da tsananin ƙarfin lantarki, tsawon rayuwa.
Alloys na jan karfe masu laushi ba sa juriya da walƙiya, jan ƙarfe na beryllium yana da ƙarfi don hana faɗuwa da wuri da samar da cikakkiyar walƙiya.Tagulla na Beryllium kuma ana iya waldar tsinkaya a kauri da ke ƙasa da 0.25mm.Kamar yadda ake yin waldi ta wurin juriya, ana amfani da kayan aikin AC galibi.
Lokacin sayar da nau'ikan karafa masu kama da juna, ƙumburi suna cikin manyan gami masu ɗaukar nauyi.Tagulla na Beryllium ba zai iya jurewa ba don naushi ko fitar da kusan kowace siffa mai dunƙulewa.Ciki har da siffofi masu kaifi sosai.Dole ne a samar da aikin aikin jan karfe na beryllium kafin maganin zafi don guje wa fashewa.
Kamar juriya tabo waldi, beryllium jan karfe tsinkaya walda tafiyar matakai akai-akai bukatar mafi girma amperage.Dole ne a yi amfani da wutar lantarki nan take kuma ya yi girma sosai don sa fitowar ta narke kafin ta tsage.Ana daidaita matsa lamba da lokacin walda don sarrafa karyewar kumbura.Matsin walda da lokaci suma sun dogara ne akan jumhuriyar juzu'i.Matsin fashewa zai rage lahanin walda kafin da bayan walda.


Lokacin aikawa: Afrilu-15-2022